ZURÜCK ZUM HUB
Technisch

Chemical Tankers: Lining Solutions using Bromobutyl Rubber for Acid Resistance.

Chemical Tankers: Lining Solutions using Bromobutyl Rubber for Acid Resistance.

Artikel teilen

Teilen Sie diesen technischen Beitrag mit Ihrem Engineering-Team.

Chemical Tankers: Lining Solutions using Bromobutyl Rubber for Acid Resistance

Problem Statement

Chemical tankers transporting concentrated acids face severe material degradation. Conventional rubbers like NBR and EPDM exhibit poor resistance to acidic environments, leading to swelling, cracking, and delamination. These failures compromise tank integrity and safety.

Material Science Analysis

Bromobutyl rubber excels in acid resistance due to its halogenated structure. The bromine groups provide superior chemical inertness, preventing acid penetration and swelling. Unlike NBR, which degrades in acidic media, Bromobutyl maintains structural integrity. Its low permeability also minimizes acid diffusion, ensuring long-term performance.

Technical Specs

  • Shore A Hardness: 50-70
  • Tensile Strength: 10-15 MPa
  • Elongation at Break: 400-600%
  • Temperature Range: -40°C to +150°C
  • Compression Set: ≤20% (70 hours at 150°C)

Material Comparison

Material Acid Resistance Temperature Range (°C) Compression Set (%) Permeability
Bromobutyl Rubber Excellent -40 to +150 ≤20 Low
NBR Poor -20 to +120 ≥50 High
EPDM Moderate -40 to +150 ≤30 Moderate

Standard Compliance

RubberQ adheres to IATF 16949 standards for batch-to-batch consistency. Our Bromobutyl formulations comply with ASTM D2000 for material callouts and ISO 3601 for sealing performance. Surface preparation and bonding processes meet ASTM D429 adhesion testing requirements.

CTA

For custom material compound development or IATF 16949 documentation, consult RubberQ’s engineering department.

Artikel teilen

Teilen Sie diesen technischen Beitrag mit Ihrem Engineering-Team.

Technische Updates abonnieren

Erhalten Sie neue Material-Insights und Engineering-Notizen per E-Mail.

Verwandte Artikel

07. Apr. 2026

Surface Blooming: Is that White Powder on your Rubber Part a Defect?

Surface Blooming: Is that White Powder on your Rubber Part a Defect? Problem Statement A white powdery residue (blooming) appears on EPDM rubber seals after 72 hours of heat aging at 150°C. The customer suspects material degradation, but the root cause is likely unreacted curing agents migrating to the surface. Material Science Analysis Primary Cause: […]

Artikel lesen

07. Apr. 2026

A-Batch Mixing: How RubberQ’s Internal Compound Development Ensures Material Purity.

A-Batch Mixing: How RubberQ’s Internal Compound Development Ensures Material Purity Problem Statement Third-party rubber compounds often introduce contamination risks, inconsistent filler dispersion, and batch-to-batch variability. These issues lead to premature seal failure in high-temperature (150°C+) or chemically aggressive environments. Material Science Analysis Contaminants (e.g., residual processing oils, cross-linked agglomerates) create weak points in vulcanized rubber. […]

Artikel lesen

06. Apr. 2026

Tolerance Grade M2: Understanding ISO 3302-1 for Precision Molded Parts.

Tolerance Grade M2: Understanding ISO 3302-1 for Precision Molded Parts Problem Statement Precision molded rubber parts often fail due to dimensional instability under high-temperature and high-pressure conditions. This leads to compression set failure and chemical degradation, particularly in applications like EV battery cooling seals and AI server manifold gaskets. Material Science Analysis Standard EPDM and […]

Artikel lesen

Benötigen Sie technische Beratung?

Unser Ingenieurteam kann Ihnen helfen, diese Materialerkenntnisse auf Ihr spezifisches Projekt anzuwenden.

ANGEBOT ANFORDERN